EN GJL 100 Cast Iron Thermal Properties ( Gray, flake graphite)
| Melting point | 1130 | – | 1200 | °C |
| Maximum service temperature | 350 | – | 450 | °C |
| Minimum service temperature | -150 | – | -50 | °C |
| Thermal conductivity | 50 | – | 72 | W/m.°C |
| Specific heat capacity | 480 | – | 520 | J/kg.°C |
| Thermal expansion coefficient | 11 | – | 13 | µstrain/°C |
| Thermal shock resistance | 58.7 | – | 94.8 | °C |
| Thermal distortion resistance | 4.12 | – | 6.11 | MW/m |
| Latent heat of fusion | 270 | – | 275 | kJ/kg |
EN GJL 100 Similar Compositions
| NBN 83001 FGG10 (Belgium) |
| NBN 83001 FGG15 (Belgium) |
| GB 9439(88) HT 100 (China) |
| DS 11301 GG10 (Denmark) |
| DS 11301 GG15 (Denmark) |
| AFNOR NFA32101 FGL150 (France) |
| AFNOR NFA32101 FGL150A (France) |
| DIN WNr 0.6010 (Germany) |
| DIN 1691 GG10 (Germany) |
| IS 210 FG150 (India) |
| UNI 5007 G10 (Italy) |
| JIS G5501(95) FC100 (Japan) |
| JIS G5501(95) FC150 (Japan) |
| NEN 6002A GG15 (Netherlands) |
| NS 722 SjG15 (Norway) |
| NS 722 SjG150 (Norway) |
| AS 1830(86) T150 (NSW Australia) |
| GOST 1412 SCh10 (Russian Federation) |
| GOST 1412 SCh15 (Russian Federation) |
| ISO 185(88) 100 (International) |
| ISO 185(88) 150 (International) |
| BS 1452 100 (United Kingdom) |
| BS 1452 150 (United Kingdom) |
| ASME SA278 20 (USA) |
| ASTM A278(93) 20 (USA) |
| ASTM A278M(93) 150 (USA) |
| ASTM A48(94) 20A (USA) |
| ASTM A48(94) 20B (USA) |
| ASTM A48(94) 20C (USA) |
| ASTM A48(94) 20S (USA) |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey