Aluminum 6005 Chemical Composition

Designation

6005, wrought
UNS numberA96005
EN nameEN AW-6005

Aluminum 6005 Chemical Composition

Al (aluminum)97.5–99%
Cr (chromium)0–0.1%
Cu (copper)0–0.1%
Fe (iron)0–0.35%
Mg (magnesium)0.4–0.6%
Mn (manganese)0–0.1%
Si (silicon)0.6–0.9%
Ti (titanium)0–0.1%
Zn (zinc)0–0.1%
Other0–0.15%

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey