Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S

Material Standards with Similar Chemical Composition |
---|
GB 1348(88) QT 450-10 (China) |
AFNOR NFA32201 FGS450-10 (France) |
JIS G5502(95) FCD45 Class 2 (Japan) |
GOST 7293 VCh45 (Russian Federation) |
SIS 140722 0722-00 (Sweden) |
ISO 1083(87) 450-10 (International) |
BS 2789 450/10 (United Kingdom) |
ASTM A536(93) 60-42-10 (USA) |
ASTM A716(95) A716 (USA) |