NBN 830-02 FNG70-2 (Belgium)NBN 830-02 FNG80-2 (Belgium)GB 1348(88) QT 700-2 (China)DS 11303 707 (Denmark)DS 11303 708 (Denmark)AFNOR NFA32201 FGS700-2 (France)AFNOR NFA32201 FGS800-2 (France)DIN WNr 0.7070 (Germany)DIN 1693 GGG-70 (Germany)IS 1865 SG700/2 (India)IS 1865 SG800/2 (India)UNI 4544 GS700-2 (Italy)UNI 4544 GS800-2 (Italy)JIS G5502(95) FCD70 Class 5 (Japan)JIS G5502(95) FCD80 Class 6 (Japan)NEN 2733 GN700-2 (Netherlands)NEN 2733 … Continue reading Cast iron, nodular graphite, EN GJS 700-2, as cast & normalized Equivalent Grades | Modulus Metal | Supplier | Foundry | Castings Products | in TURKEY