EN GJL 150 Chemical Composition:
Base Fe (Iron) : Fe/3.2C/2.6Si/0.6Mn/0.1P/<0.15S
Element | Min (%) | Max (%) |
---|---|---|
C (Carbon) | 3.2 | 3.2 |
Fe (Iron) | 93.4 | 93.5 |
Mn (Manganese) | 0.6 | 0.6 |
P (Phosphorus) | 0.1 | 0.1 |
S (Sulfur) | 0 | 0.15 |
Si (Silicon) | 2.6 | 2.6 |