Base Fe (Iron) : Fe/3.6-4C/2.4-2.6Si/0.5-0.7Mn/trace P, S
Element | Min (%) | Max (%) |
---|
C (Carbon) | 3.6 | 4.0 |
Fe (Iron) | 92.7 | 93.5 |
Mn (Manganese) | 0.5 | 0.7 |
P (Phosphorus) | 1e-9 | 1e-9 |
S (Sulfur) | 1e-9 | 1e-9 |
Si (Silicon) | 2.4 | 2.6 |
EN GJL 100 Chemical Composition | | |
Material Standards with Similar Chemical Composition |
---|
NBN 83001 FGG10 (Belgium) |
NBN 83001 FGG15 (Belgium) |
GB 9439(88) HT 100 (China) |
DS 11301 GG10 (Denmark) |
DS 11301 GG15 (Denmark) |
AFNOR NFA32101 FGL150 (France) |
AFNOR NFA32101 FGL150A (France) |
DIN WNr 0.6010 (Germany) |
DIN 1691 GG10 (Germany) |
IS 210 FG150 (India) |
UNI 5007 G10 (Italy) |
JIS G5501(95) FC100 (Japan) |
JIS G5501(95) FC150 (Japan) |
NEN 6002A GG15 (Netherlands) |
NS 722 SjG15 (Norway) |
NS 722 SjG150 (Norway) |
AS 1830(86) T150 (NSW Australia) |
GOST 1412 SCh10 (Russian Federation) |
GOST 1412 SCh15 (Russian Federation) |
ISO 185(88) 100 (International) |
ISO 185(88) 150 (International) |
BS 1452 100 (United Kingdom) |
BS 1452 150 (United Kingdom) |
ASME SA278 20 (USA) |
ASTM A278(93) 20 (USA) |
ASTM A278M(93) 150 (USA) |
ASTM A48(94) 20A (USA) |
ASTM A48(94) 20B (USA) |
ASTM A48(94) 20C (USA) |
ASTM A48(94) 20S (USA) |
EN GJL 100 Chemical Composition (Cast iron, gray, flake graphite)