EN GJS 700-2 as cast & normalized, nodular graphite, Mechanical Properties |
---|
Young’s modulus 172 – 180 GPa |
Flexural modulus * 172 – 180 GPa |
Shear modulus 67 – 71 GPa |
Bulk modulus 124 – 137 GPa |
Poisson’s ratio 0.27 – 0.28 |
Shape factor 21 |
Yield strength (elastic limit) 416 – 471 MPa |
Tensile strength 700 – 800 MPa |
Compressive strength * 425 – 480 MPa |
Flexural strength (modulus of rupture) 416 – 471 MPa |
Elongation 2 – 5 % strain |
Hardness – Vickers 250 – 270 HV |
Fatigue strength at 10^7 cycles 280 – 304 MPa |
Fatigue strength model (stress range) 188 – 234 MPa Parameters: Stress Ratio = 0, Number of Cycles = 1e7 |
Fracture toughness 22 – 34 MPa.m^0.5 |
Mechanical loss coefficient (tan delta) * 8e-4 – 0.0012 |
*Values are approximations. This information’s accuracy is not guaranteed. |