Base Fe (Iron) : Fe/3.3-3.8C/2-3Si/<1.0Ni/0.2-0.5Mn/0.02-0.07Mg Material Standards with Similar Chemical Composition NBN 830-02 FNG70-2 (Belgium) NBN 830-02 FNG80-2 (Belgium) GB 1348(88) QT 700-2 (China) DS 11303 707 (Denmark) DS 11303 708 (Denmark) AFNOR NFA32201 FGS700-2 (France) AFNOR NFA32201 FGS800-2 (France) DIN WNr 0.7070 (Germany) DIN 1693 GGG-70 (Germany) IS 1865 SG700/2 (India) IS 1865 SG800/2 … Continue reading EN GJS 700-2, as cast & normalized, Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY