EN GJL 100 Mechanical Properties
EN GJL 100 Cast iron, gray, flake graphite, Mechanical Properties |
---|
Young’s modulus * 80 – 100 GPa |
Flexural modulus * 80 – 100 GPa |
Shear modulus * 31 – 40 GPa |
Bulk modulus * 54 – 71 GPa |
Poisson’s ratio 0.255 – 0.265 |
Shape factor 25 |
Yield strength (elastic limit) 65 – 98 MPa |
Tensile strength 100 – 200 MPa |
Compressive strength * 130 – 200 MPa |
Flexural strength (modulus of rupture) * 75 – 115 MPa |
Elongation * 0.5 – 0.7 % strain |
Hardness – Vickers 90 – 216 HV |
Fatigue strength at 10^7 cycles 40 – 68 MPa |
Fatigue strength model (stress range) * 22.2 – 61.4 MPa Parameters: Stress Ratio = 0, Number of Cycles = 1e7 |
Fracture toughness * 20 – 24 MPa.m^0.5 |
Mechanical loss coefficient (tan delta) 0.01 – 0.035 |
*Values are approximations. This information’s accuracy is not guaranteed. |
Standard/Organization | Designation |
---|---|
BS EN 1561:1997 | EN GJL 100 |
BS 1542:1990 | BS Grade 100 |
UNS Number | F11401 |
DIN WNr | 0.6010 |
DIN 1691 | GG10 |
EN GJL 100 Cast Iron Designation |