Cast iron, gray, flake graphite, EN GJL 300 Equivalent Grades | Modulus Metal | Supplier | Foundry | Castings Products | in TURKEY

Ingot Casting_Gray Cast Iron Microstucture Foundry Supplier Parts Products Exporter Manufacturing in Turkey

EN GJL 300 Equivalent Grades

StandardDesignationCountry
BS EN 1561:1997EN GJL 300International
BS 1542:1990BS Grade 300United Kingdom
UNS NumberF13101International
DIN WNr0.6030Germany
DIN 1691GG30Germany
NBN 83001FGG30Belgium
GB 9439(88)HT 300China
DS 11301GG30Denmark
AFNOR NFA32101FGL300France
ISO 185(88)300International
BS 1452300United Kingdom
IS 210FG300India
UNI 5007G30Italy
JIS G5501(95)FC300Japan
NEN 6002AGG30Netherlands
NS 722SjG30Norway
AS 1830(86)T300Australia (NSW)
GOST 1412SCh30Russian Federation
SABS 1034300South Africa
ASTM A278M(93)300USA
EN GJL 300 Equivalent Grades

Standards with similar compositions:

AFNOR NFA32101 FGL350A (France)

AFNOR NFA32101 FGL400A (France)

DIN WNr 0.6025 (Germany)

DIN 1691 GG25 (Germany)

NS 722 SjG350 (Norway)

AS 1830(86) T300 (NSW Australia)

ASME SA278 45 (USA)

ASTM A278(93) 45 (USA)

ASTM A278M(93) 325 (USA)

ASTM A48(94) 45A (USA)

ASTM A48(94) 45B (USA)

ASTM A48(94) 45C (USA)