Base Fe (Iron) : Fe/3.2C/2.6Si/0.6Mn/0.1P/<0.15S

Material Standards with Similar Chemical Composition |
---|
GB 9439(88) HT 150 (China) |
AFNOR NFA32101 FGL200A (France) |
AFNOR NFA32101 FGL250A (France) |
DIN WNr 0.6015 (Germany) |
DIN 1691 GG15 (Germany) |
UNI 5007 G15 (Italy) |
NS 722 SjG200 (Norway) |
AS 1830(86) T180 (NSW Australia) |
GOST 1412 SCh18 (Russian Federation) |
SS 140115 115 (Sweden) |
BS 1452 180 (United Kingdom) |
ASME SA278 25 (USA) |
ASTM A278(93) 25 (USA) |
ASTM A278M(93) 175 (USA) |
ASTM A48(94) 25A (USA) |
ASTM A48(94) 25B (USA) |
ASTM A48(94) 25C (USA) |
ASTM A48(94) 25S (USA) |