PA610 (Polyamide 610 / Nylon 610)

PA610 (Polyamide 610 / Nylon 610)

PA610 Strengths

PA610 (nylon 610) absorbs roughly half as much water as PA6 and PA66, which gives better dimensional stability and steadier electrical properties. It stays tough to very low temperatures and is stronger than PA6/12, PA12 and PA11.

PA610 Limitations

Strength is lower than PA6 or PA66, cost is higher, and mold shrinkage is high.

PA610 Designation

PA610, also written 6.10 or 6/10.

Typical Uses of PA610

Electrical insulation and components similar to those made from PA6 and PA66 where lower moisture uptake justifies the higher price, such as zip fasteners, insulators, precision parts and brush filaments.

PA610 Compositional Summary

(NH(CH2)6NHCO(CH2)8CO)n. The renewable part comes from sebacic acid, obtained from castor oil.
Material familyPlastic (thermoplastic, semi-crystalline)
Base materialPA610 (Polyamide / nylon 610)
CAS number9011-52-3

PA610 Parts from Turkey

Looking for PA610 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA610 parts in-house and inspects them before shipment.

PA610 Grades

PA610 Unfilled Grades

PA610 Unfilled Grade Material Data Sheet

PA610 Glass Filled Grades

PA610 30-40% Glass Fiber Material Data Sheet