PA610 30-40% Glass Fiber Material Data Sheet

PA610 30-40% Glass Fiber (Polyamide 610) Material Data Sheet

PA610 30-40% Glass Fiber Overview

PA610 30-40% glass fiber is a grade of polyamide 610 (PA610, nylon 610), designated Polyamide (Nylon) (Type 610, 30-40% Glass Fiber). This PA610 30-40% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA610 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA610 parts in-house and inspects them before shipment.

PA610 30-40% Glass Fiber Designation

Polyamide (Nylon) (Type 610, 30-40% Glass Fiber)
TradenamesLNP Thermocomp, Nylene, Ultramid

PA610 30-40% Glass Fiber Typical uses

Zip fasteners, electrical insulators, precision parts, filaments for brushes.

PA610 30-40% Glass Fiber Composition detail

Polymer60–70%
Glass (fiber)30–40%

PA610 30-40% Glass Fiber Physical properties

Density1.33–1.36g/cm3

PA610 30-40% Glass Fiber Mechanical properties

Young’s modulus5.74–7.16GPa
Specific stiffness4.27–5.33MN.m/kg
Yield strength (elastic limit)97.9–122MPa
Tensile strength115–140MPa
Specific strength72.8–90.8kN.m/kg
Elongation5.64–8.11% strain
Elongation at yield4.74–9.01% strain
Compressive modulus6.13–6.77GPa
Compressive strength145–161MPa
Flexural modulus5.87–7.03GPa
Flexural strength (modulus of rupture)167–204MPa
Shear modulus2.28–2.39GPa
Shear strength68.9–84.2MPa
Bulk modulus8.65–9.57GPa
Poisson’s ratio0.367–0.382 
Shape factor5.81
Hardness – Vickers31–35HV
Hardness – Rockwell M163–180 
Hardness – Rockwell R163–180 
Hardness – Shore D93–97 
Elastic stored energy (springs)739–1170kJ/m3
Fatigue strength at 10^7 cycles48.5–53.6MPa

PA610 30-40% Glass Fiber Impact & fracture properties

Fracture toughness4.46–4.93MPa.m0.5
Toughness (G)2.97–3.96kJ/m2
Impact strength, notched 23 °C11.2–21.8kJ/m2
Impact strength, unnotched 23 °C77–113kJ/m2

PA610 30-40% Glass Fiber Thermal properties

Melting point210–230°C
Glass temperature44–56°C
Heat deflection temperature 0.45MPa198–246°C
Heat deflection temperature 1.8MPa210–213°C
Maximum service temperature90–120°C
Minimum service temperature-64–-44°C
Thermal conductivity0.365–0.38W/m.°C
Specific heat capacity1410–1470J/kg.°C
Thermal expansion coefficient39.6–40.4µstrain/°C
Thermal shock resistance366–497°C
Thermal distortion resistance0.00912–0.00953MW/m

PA610 30-40% Glass Fiber Electrical properties

Electrical resistivity2.73e21–6.83e22µohm.cm
Electrical conductivity2.52e-21–6.32e-20%IACS
Dielectric constant (relative permittivity)4.57–6.44 
Dissipation factor (dielectric loss tangent)0.0223–0.0587 
Dielectric strength (dielectric breakdown)20.4–34.7MV/m
Comparative tracking index600  V

PA610 30-40% Glass Fiber Magnetic properties

Magnetic typeNon-magnetic

PA610 30-40% Glass Fiber Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2060–2310m/s
Mechanical loss coefficient (tan delta)0.0099–0.0109 

PA610 30-40% Glass Fiber Absorption & permeability

Water absorption @ 24 hrs0.41–0.67%
Water absorption @ sat1.8–2.4%
Humidity absorption @ sat1–1.4%

PA610 30-40% Glass Fiber Processing properties

Polymer injection moldingExcellent
Polymer extrusionAcceptable
Polymer thermoformingLimited use
Linear mold shrinkage1.5 – 4 %
Melt temperature213 – 288 °C
Mold temperature60 – 100 °C
Molding pressure range6.88 – 131 MPa

PA610 30-40% Glass Fiber Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning