Home » PA (Polyamide / Nylon) » PA610 (Polyamide 610 / Nylon 610) » PA610 Unfilled Grades » PA610 Unfilled Grade Material Data Sheet
PA610 Unfilled Grade (Polyamide 610) Material Data Sheet
PA610 Unfilled Grade Overview
PA610 unfilled grade is a grade of polyamide 610 (PA610, nylon 610), designated Polyamide (Nylon) (Type 610, Molding and Extrusion). This PA610 unfilled grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA610 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA610 parts in-house and inspects them before shipment.
PA610 Unfilled Grade Designation
Polyamide (Nylon) (Type 610, Molding and Extrusion) Tradenames Akromid, Amilan, Badamid, Grilamid, Hiprolon, Isocor, Nylene, Shandong, Technyl Exten, Terez, Ultramid, Vestamid, Zytel
PA610 Unfilled Grade Typical uses
Zip fasteners, electrical insulators, precision parts, filaments for brushes.
PA610 Unfilled Grade Composition detail
PA610 Unfilled Grade Physical properties
PA610 Unfilled Grade Mechanical properties
Young’s modulus 1.45 – 1.8 GPa Specific stiffness 1.35 – 1.68 MN.m/kg Yield strength (elastic limit) 44.5 – 55.5 MPa Tensile strength 56.6 – 69.2 MPa Specific strength 41.6 – 51.9 kN.m/kg Elongation 41 – 59 % strain Elongation at yield 15.2 – 28.8 % strain Compressive modulus 1.54 – 1.71 GPa Compressive strength 71.7 – 79.3 MPa Flexural modulus 1.48 – 1.77 GPa Flexural strength (modulus of rupture) 75.7 – 92.5 MPa Shear modulus 0.566 – 0.595 GPa Shear strength 34 – 41.5 MPa Bulk modulus 2.57 – 2.84 GPa Poisson’s ratio 0.35 – 0.4 Shape factor 4.3 Hardness – Vickers 14 – 16 HV Hardness – Rockwell M 114 – 126 Hardness – Rockwell R 114 – 126 Hardness – Shore D 81 – 84 Elastic stored energy (springs) 607 – 963 kJ/m3 Fatigue strength at 10^7 cycles 23.9 – 26.4 MPa
PA610 Unfilled Grade Impact & fracture properties
Fracture toughness 3.37 – 3.73 MPa.m0.5 Toughness (G) 6.74 – 8.98 kJ/m2 Impact strength, notched 23 °C 5.57 – 10.8 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
PA610 Unfilled Grade Thermal properties
Melting point 210 – 230 °C Glass temperature 44 – 56 °C Heat deflection temperature 0.45MPa 157 – 173 °C Heat deflection temperature 1.8MPa 76 – 84 °C Maximum service temperature 90 – 120 °C Minimum service temperature -64 – -44 °C Thermal conductivity 0.2 – 0.22 W/m.°C Specific heat capacity 1540 – 1590 J/kg.°C Thermal expansion coefficient 139 – 141 µstrain/°C Thermal shock resistance 189 – 256 °C Thermal distortion resistance 0.00143 – 0.00157 MW/m
PA610 Unfilled Grade Electrical properties
Electrical resistivity 1.32e19 – 3.3e20 µohm.cm Electrical conductivity 5.22e-19 – 1.31e-17 %IACS Dielectric constant (relative permittivity) 4.26 – 6.01 Dissipation factor (dielectric loss tangent) 0.0431 – 0.114 Dielectric strength (dielectric breakdown) 23.5 – 40.1 MV/m Comparative tracking index 600 V
PA610 Unfilled Grade Magnetic properties
Magnetic type Non-magnetic
PA610 Unfilled Grade Optical, aesthetic and acoustic properties
Refractive index 1.56 – 1.57 Transparency Translucent Acoustic velocity 1160 – 1300 m/s Mechanical loss coefficient (tan delta) 0.0197 – 0.0218
PA610 Unfilled Grade Absorption & permeability
Water absorption @ 24 hrs 0.78 – 1.3 % Water absorption @ sat 3.4 – 4.6 % Humidity absorption @ sat 1.2 – 1.6 %
PA610 Unfilled Grade Processing properties
Polymer injection molding Excellent Polymer extrusion Acceptable Polymer thermoforming Limited use Linear mold shrinkage 0.5 – 1.5 % Melt temperature 229 – 260 °C Mold temperature 30 – 60 °C Molding pressure range 6.88 – 131 MPa
PA610 Unfilled Grade Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning
PA610 Grades
PA610 Unfilled Material Data Sheets
Unfilled Unfilled You are here
All PA610 Grades
Modulus Metal Services