| UNS number | F45004 |
Designation
BS EN 12513:2011 EN GJN HV600 (XCr11) (former BS 3F). Record based on BS 4844:1986 BS grade 3F.
Standards with similar compositions:
| AFNOR NFA32401 FBCr12MoNi (France) |
| BS 4844 3F (United Kingdom) |
| BS 4844 3G (United Kingdom) |
| ASTM A532/A532M(93a) 12% Cr (USA) |
Typical uses
Abrasion resistant components, typically in mineral-pulverizing mills, e.g. grinding balls, drum liner plates, spiral classifier-shoes, pulverizing-bars.