EN GJN HV600 (XCr11) Chemical Composition, former BS 3F, Cast iron, white, high-chromium alloy
Compositional summary Fe73-87 / Cr11-14 / C1.8-3.6 / Mn0.15-1.5 (impurities: Mo<3, Cu<2, Ni<2, Si<1, P<0.1, S<0.1) Material family: Metal (ferrous) Base material: Fe (Iron) Elements Min Max % C (carbon) 1.8 – 3.6 % Cr (chromium) 11 – 14 % Cu (copper) 0 – 2 % Fe (iron) 72.8 – 87.1 … Continue reading EN GJN HV600 (XCr11) Chemical Composition, former BS 3F, Cast iron, white, high-chromium alloy