Designation
BS EN 12513:2011 EN GJN HV350 (former BS 1A). Record based on BS 4844:1986 BS grade 1A.
Tradenames: CY/A, CY/H, MEEHANITE WEC
Standards with similar compositions:
| France: | FBA to AFNOR NF A32-401, FBO to AFNOR NF A32-401 |
| India: | Grade 1 to IS 7925, Grade 3 to IS 7925 |
| UK: | 1A to BS 4844, 1C to BS 4844, EN-GJN-HV350 to BS EN 12513 |
Typical uses
Abrasion resistant components.