EN GJN HV350, former BS 1A, Mechanical Properties, Cast iron, white, low alloy

Designation BS EN 12513:2011 EN GJN HV350 (former BS 1A). Record based on BS 4844:1986 BS grade 1A. Tradenames: CY/A, CY/H, MEEHANITE WEC EN GJN HV350 Mechanical Properties, former BS 1A, Cast iron, white, low alloy: EN GJN HV350, former BS 1A, Mechanical Properties Min Max Young’s modulus *185 215 GPa Specific stiffness *24 28 … Continue reading EN GJN HV350, former BS 1A, Mechanical Properties, Cast iron, white, low alloy