EN GJN HV350 Chemical Composition, former BS 1A, Cast iron, white, low alloy
Designation BS EN 12513:2011 EN GJN HV350 (former BS 1A). Record based on BS 4844:1986 BS grade 1A. Tradenames: CY/A, CY/H, MEEHANITE WEC Compositional summary: Fe92-97 / C2.4-3.9 / Si0.4-1.5 / Mn0.2-1 (impurities: Cr<2, P<0.15) Material Family: Metal (ferrous) Base material: Fe (Iron) EN GJN HV350 Chemical Composition, former BS 1A, Cast iron, white, low … Continue reading EN GJN HV350 Chemical Composition, former BS 1A, Cast iron, white, low alloy