| Designation | |
| CuAl10Fe3 | |
| UNS number | C95200 |
| EN name | CC331G |
| ISO name | CuAl10FE3 |
| GB (Chinese) name | CuAl10Fe3 |
| JIS (Japanese) name | Al BC 1 |
Bronze CuAl10Fe3 Mechanical Properties (C95200, cast aluminum bronze)
| Young’s modulus | 100 | – | 103 | GPa |
| Specific stiffness | 13.1 | – | 13.5 | MN.m/kg |
| Yield strength (elastic limit) | 170 | – | 200 | MPa |
| Tensile strength | 500 | – | 590 | MPa |
| Specific strength | 22.2 | – | 26.2 | kN.m/kg |
| Elongation | 18 | – | 40 | % strain |
| Compressive strength | 170 | – | 200 | MPa |
| Flexural modulus | 100 | – | 103 | GPa |
| Flexural strength (modulus of rupture) | 170 | – | 200 | MPa |
| Shear modulus | 37 | – | 38.1 | GPa |
| Bulk modulus | 108 | – | 111 | GPa |
| Poisson’s ratio | 0.34 | – | 0.35 | |
| Shape factor | 28 | |||
| Hardness – Vickers | 90 | – | 140 | HV |
| Elastic stored energy (springs) | 143 | – | 196 | kJ/m^3 |
| Fatigue strength at 10^7 cycles | 204 | – | 228 | MPa |
| Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles | 177 | – | 263 | MPa |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey