| Designation | |
| CuAl10Fe3 | |
| UNS number | C95200 |
| EN name | CC331G |
| ISO name | CuAl10FE3 |
| GB (Chinese) name | CuAl10Fe3 |
| JIS (Japanese) name | Al BC 1 |
Bronze CuAl10Fe3 Chemical Composition (C95200, cast aluminum bronze)
| Al (aluminum) | 8.5 | – | 9.5 | % |
| Cu (copper) | 86.5 | – | 89 | % |
| Fe (iron) | 2.5 | – | 4 | % |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey