Bronze CuAl10Fe3 Chemical Composition (C95200, cast aluminum bronze)

Designation CuAl10Fe3 UNS number C95200 EN name CC331G ISO name CuAl10FE3 GB (Chinese) name CuAl10Fe3 JIS (Japanese) name Al BC 1 Bronze CuAl10Fe3 Chemical Composition (C95200, cast aluminum bronze) Al (aluminum) 8.5 – 9.5 % Cu (copper) 86.5 – 89 % Fe (iron) 2.5 – 4 % MODULUS METALSand Casting in Turkey, Permanent Mold Casting in … Continue reading Bronze CuAl10Fe3 Chemical Composition (C95200, cast aluminum bronze)