Bronze CuAl10Fe3 Mechanical Properties (C95200, cast aluminum bronze)

Designation CuAl10Fe3 UNS number C95200 EN name CC331G ISO name CuAl10FE3 GB (Chinese) name CuAl10Fe3 JIS (Japanese) name Al BC 1 Bronze CuAl10Fe3 Mechanical Properties (C95200, cast aluminum bronze) Young’s modulus 100 – 103 GPa Specific stiffness 13.1 – 13.5 MN.m/kg Yield strength (elastic limit) 170 – 200 MPa Tensile strength 500 – 590 MPa … Continue reading Bronze CuAl10Fe3 Mechanical Properties (C95200, cast aluminum bronze)