Compositional summary
Al99.5-100 (impurities: Other<0.5)
| Material family | Metal (non-ferrous) |
| Base material | Al (Aluminum) |
Composition detail
| Al (aluminum) | 99.5 | 100 | % |
| Other | 0 | 0.5 | % |
Aluminum S150.1: LM0-M Composition | UNS A01501 Composition
Aluminum, commercial purity, S150.1 : LM0-M, cast | Designation
Aluminum S150.1: LM0-M | Composition
Aluminum S150.1: LM0-M | Mechanical Properties
Aluminum S150.1: LM0-M | Equivalent Grades