Aluminum A360.0 Thermal Properties (Die cast, F)

Aluminum A360.0 Thermal Properties

Melting point549–604°C
Maximum service temperature150–170°C
Minimum service temperature-273  °C
Thermal conductivity141–152W/m.°C
Specific heat capacity944–982J/kg.°C
Thermal expansion coefficient20.5–21.6µstrain/°C
Thermal shock resistance104–117°C
Thermal distortion resistance6.63–7.29MW/m
Latent heat of fusion384–393kJ/kg

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treatment, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey