Aluminum A360.0 Designation (Die cast, F)
Aluminum A360.0 Designation (Die cast, F) A360.0 (Aluminum Association) Condition F (As-fabricated) UNS number A13600 EN number EN AC-43100 / EN AC-Al Si10Mg MODULUS METALSand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( … Continue reading Aluminum A360.0 Designation (Die cast, F)