Aluminum A360.0 Mechanical Properties (Die cast, F)

Aluminum A360.0 Mechanical Properties Young’s modulus 69.6 – 72.4 GPa Specific stiffness 25.9 – 27 MN.m/kg Yield strength (elastic limit) 157 – 173 MPa Tensile strength 317 – 349 MPa Specific strength 58.3 – 64.6 kN.m/kg Elongation 5 – 6 % strain Compressive strength 157 – 173 MPa Flexural modulus 69.6 – 72.4 GPa Flexural … Continue reading Aluminum A360.0 Mechanical Properties (Die cast, F)