Aluminum, A201.0, cast, T7 | Mechanical Properties

Mechanical Properties of Aluminum, A201.0, cast, T7

Young’s Modulus7174.6GPa
Specific Stiffness25.426.7MN·m/kg
Yield Strength (Elastic Limit)331366MPa
Tensile Strength386427MPa
Specific Strength118131kN·m/kg
Elongation1.55.0% strain
Compressive Strength338374MPa
Flexural Modulus7174.6GPa
Flexural Strength (Modulus of Rupture)331366MPa
Shear Modulus2829.4GPa
Bulk Modulus69.673.2GPa
Poisson’s Ratio0.330.343—
Shape Factor20——
Hardness – Vickers148152HV
Elastic Stored Energy (Springs)752920kJ/m³
Fatigue Strength at 10⁷ Cycles9799MPa
Fatigue Strength Model (Stress Range)88.6108MPa
Mechanical Properties of UNS A12010

MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey