Composition Overview
| Attribute | Details |
|---|---|
| Compositional Summary | Al93-95 / Cu4-5 / Ag0.4-1 / Mn0.2-0.4 / Mg0.15-0.35 / Ti0.15-0.35 (Impurities: Fe<0.1, Si<0.05, Other<0.1) |
| Material Family | Metal (non-ferrous) |
| Base Material | Al (Aluminum) |
| Aluminum, A201.0, cast, T7 Composition UNS A12010 Composition |
Composition Details
| Element | Min (%) | Max (%) |
|---|---|---|
| Ag (Silver) | 0.4 | 1.0 |
| Al (Aluminum) | 92.6 | 95.1 |
| Cu (Copper) | 4.0 | 5.0 |
| Fe (Iron) | 0.0 | 0.1 |
| Mg (Magnesium) | 0.15 | 0.35 |
| Mn (Manganese) | 0.2 | 0.4 |
| Si (Silicon) | 0.0 | 0.05 |
| Ti (Titanium) | 0.15 | 0.35 |
| Other | 0.0 | 0.1 |
| Aluminum, A201.0, cast, T7 Chemical Composition UNS A12010 Chemical Composition |
Aluminum, A201.0, cast, T7 | General information
Aluminum, A201.0, cast, T7 | Composition
Aluminum, A201.0, cast, T7 | Mechanical Properties
Aluminum, A201.0, cast, T7 Equivalent | Grades