| Property | Value Range | Units |
|---|---|---|
| Young’s modulus | 71.5 – 74.5 | GPa |
| Specific stiffness | 26.6 – 27.8 | MN·m/kg |
| Yield strength (elastic limit) | 164 – 182 | MPa |
| Tensile strength | 235 – 259 | MPa |
| Specific strength | 61 – 67.8 | kN·m/kg |
| Elongation | 2.9 – 3.4 | % strain |
| Compressive strength | 105 – 116 | MPa |
| Flexural modulus | 71.5 – 74.5 | GPa |
| Flexural strength (modulus of rupture) | 164 – 182 | MPa |
| Shear modulus | 26.7 – 28.2 | GPa |
| Bulk modulus | 66.9 – 76.6 | GPa |
| Poisson’s ratio | 0.322 – 0.338 | |
| Shape factor | 34 | |
| Hardness – Vickers | 89 – 105 | HV |
| Elastic stored energy (springs) | 184 – 227 | kJ/m³ |
| Fatigue strength at 10⁷ cycles | 81 – 99 | MPa |
| Fatigue strength model (stress range) | 78.2 – 103 | MPa |