Aluminum 356.0 permanent mold cast T6 General Information
| Property | Value |
|---|---|
| Designation | 356.0 (Aluminum Association) |
| Condition | T6 (Solution heat-treated and artificially aged) |
| UNS Number | A03560 |
| EN Number | EN AC-42000 / EN AC-Al Si7Mg |
Aluminum 356.0 permanent mold cast T6 General Information
Aluminum 356.0 permanent mold cast T6 Typical Uses
| Typical Uses |
|---|
| Space frames |
| Wheels |
| Axle and differential housings |
| Pumps |
| Meters |
| Differential housings |
| Intake manifolds |
| Electronic cases |
| Fuel pumps |
| Aluminum 356.0 permanent mold cast T6 Typical Uses |
MODULUS METAL
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey