Alloy 904L, wrought
ConditionAnnealed
UNS numberN08904
US nameAISI 904L, ASTM 904L
EN name~X1NiCrMoCu25-20-5
EN number~1.4539
TradenamesURANUS B6, FO 25-20 U., NAS 255, SOUDINOX B6

AISI 904L Similar Compositions

International: X1NiCrMoCu25-20-5 to ISO 16143-1, X1NiCrMoCu25-20-5 to ISO 16143-2, X1NiCrMoCu25-20-5 to ISO 16143-3, X1NiCrMoCu25-20-5 to ISO 9328-7, X2NiCrMoCu25-20-5 to ISO 9327-5
Japan: SUS317J5L to JIS G4303, SUS317J5L to JIS G4305, SUS890L to JIS G4303, SUS890L to JIS G4304, SUS890L to JIS G4305, SUS890LTB to JIS G3463, SUS890LTP to JIS G3459
Romania: 2CuMoCrNi250 to STAS 3583
South Korea: STS 890L to KS D 3706, STS890L to KS D 3698, STS890L to KS D 3705
Sweden: 2562 to SS 142562
UK: 904S13 to BS 1501/3, 904S14 to BS 1554, X1NiCrMoCu25-20-5 to BS EN 10088-1, X1NiCrMoCu25-20-5 to BS EN 10088-2, X1NiCrMoCu25-20-5 to BS EN 10088-3, X1NiCrMoCu25-20-5 to BS EN 10216-5, X1NiCrMoCu25-20-5 to BS EN 10250-4, X1NiCrMoCu25-20-5 to BS EN 10272, X1NiCrMoCu25-20-5 to BS EN 10296-2, X1NiCrMoCu25-20-5 to BS EN 10297-2
USA: F904L to ASTM A182/A182M, N08904 to ASTM A240/A240M, N08904 to ASTM A249/A249M, N08904 to ASTM A312/A312M, N08904 to ASTM B625, N08904 to ASTM B649, N08904 to ASTM B673, N08904 to ASTM B674, N08904 to ASTM B677, N08904 to SAE J405, UNS N08904

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey