AISI 904L Stainless Steel Mechanical Properties
AISI 904L Stainless Steel Mechanical Properties Young’s modulus 191 – 197 GPa Specific stiffness 24 – 24.7 MN.m/kg Yield strength (elastic limit) 257 – 284 MPa Tensile strength 575 – 635 MPa Specific strength 32.2 – 35.6 kN.m/kg Elongation 46.3 – 53.8 % strain Compressive strength 257 – 284 MPa Flexural modulus 191 – 197 … Continue reading AISI 904L Stainless Steel Mechanical Properties