AISI 904L Stainless Steel Composition

AISI 904L Stainless Steel Composition C (carbon) 0 – 0.02 % Cr (chromium) 19 – 23 % Cu (copper) 1 – 2 % Fe (iron) 38.8 – 53 % Mn (manganese) 0 – 2 % Mo (molybdenum) 4 – 5 % N (nitrogen) 0 – 0.1 % Ni (nickel) 23 – 28 % P (phosphorus) … Continue reading AISI 904L Stainless Steel Composition