C (carbon)0.33–0.38%
Cr (chromium)0.8–1.1%
Fe (iron)96.9–97.9%
Mn (manganese)0.7–0.9%
Mo (molybdenum)0.15–0.25%
P (phosphorus)0–0.035%
S (sulfur)0–0.04%
Si (silicon)0.15–0.35%
AISI 4135 Low alloy steel (4100 Series, Cr-Mo Alloyed, 0.35% C )
UNS numberG41350
US nameSAE 4137, SAE 4135H, SAE 4135, SAE 17-22-A S, ASTM L7M, ASTM L7B, ASTM G41370, ASTM G55, ASTM F70, ASTM F65, ASTM  B1, ASTM 4137, ASTM 4130H, ASTM 4130, ~SAE 4130, ~ASTM H  70, ~ASTM H65, ~ASTM H55, ~ASTM G41300, ~ASTM G70, ~ASTM G65, ~ASTM 4130
EN name~34CrMo4
EN number~1.7226, ~1.722
ISO name34CrMoS4, 33CrAlMo5-4, ~34CrMo4

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey