| AISI 4135 Low alloy steel (4100 Series, Cr-Mo Alloyed, 0.35% C ) | Equivalent Grades |
|---|---|
| UNS number | G41350 |
| US name | SAE 4137, SAE 4135H, SAE 4135, SAE 17-22-A S, ASTM L7M, ASTM L7B, ASTM G41370, ASTM G55, ASTM F70, ASTM F65, ASTM B1, ASTM 4137, ASTM 4130H, ASTM 4130, ~SAE 4130, ~ASTM H 70, ~ASTM H65, ~ASTM H55, ~ASTM G41300, ~ASTM G70, ~ASTM G65, ~ASTM 4130 |
| EN name | ~34CrMo4 |
| EN number | ~1.7226, ~1.722 |
| ISO name | 34CrMoS4, 33CrAlMo5-4, ~34CrMo4 |
Tradenames of AISI 4135 Low alloy steel (4100 Series, Cr-Mo Alloyed, 0.35% C ): 35 CR MO 4, ABRASALLOY, ASCOMETAL 35CD4, BOHLER V330, DF 38 CR MO 4, DIRO-34 CRMO 4, FAGERSTA C 643, FORTUNA TCM04, HEVA-DF-100, KRUPP 2330, KRUPP 34 CRMOS 4, POMPEY KD 33, STEEL 34 CR MO 4, TKS 34CRMO4, WITTEN KV 32 COL
| Standards with similar compositions: |
|---|
| IAS IRAM 4133 (Argentina) |
| NBN 253-02 34CrMo4 (Belgium) |
| BDS 6354 35ChM (Bulgaria) |
| GB 3077(88) 35CrMo (China) |
| GB 6478(86) ML35CrMo (China) |
| GB 8162(87) 35CrMo (China) |
| GB/T 3078(94) 35CrMo (China) |
| YB/T 5132(93) 35CrMo (China) |
| SFS 458(73) SFS458 (Finland) |
| SFS 459 Co.35Cr1.1Mo0.20 (Finland) |
| AFNOR NFA35552 34CD4 (France) |
| AFNOR NFA35552 35CD4 (France) |
| AFNOR NFA35553 35CD4 (France) |
| AFNOR NFA35556(84) 34CD4 (France) |
| AFNOR NFA35556(84) 35CD4 (France) |
| AFNOR NFA35557(83) 34CD4 (France) |
| AFNOR NFA36102(93) 30MnB5RR (France) |
| AFNOR NFA36102(93) 34CrMo4RR (France) |
| AFNOR NFA36102(93) 35B3RR (France) |
| DIN 33CrMo4 (Germany) |
| DIN WNr 1.7231 (Germany) |
| DIN 1652(90) 34CrMoS4 (Germany) |
| DIN 1652(90) WNr 1.7220 (Germany) |
| DIN 1652(90) WNr 1.7226 (Germany) |
| DIN EN 10083(91) 34CrMo4 (Germany) |
| DIN EN 10083(91) WNr 1.7220 (Germany) |
| MSZ 61(85) CMo3 (Hungary) |
| MSZ 61(85) CMo3E (Hungary) |
| MSZ 6251(87) CMo3Z (Hungary) |
| UNI 6403(86) 35CrMo4 (Italy) |
| UNI 6929(71) 35CrMo4F (Italy) |
| UNI 7356(74) 34CrMo4KB (Italy) |
| UNI 7845(78) 35CrMo4 (Italy) |
| UNI 7874(79) 35CrMo4 (Italy) |
| JIS G3311(88) SCM3M (Japan) |
| JIS G4105(79) SCM 3 (Japan) |
| JIS G4105(79) SCM435 (Japan) |
| DGN B-203 4135 (Mexico) |
| NMX-B-300(91) 4135 (Mexico) |
| NS CrMoII (Norway) |
| PNH84030 35HM (Poland) |
| PNH84030 35HMA (Poland) |
| STAS 791 33MoCr11 (Romania) |
| STAS 791 35MoCr11 (Romania) |
| STAS 791 36MoCr10 (Romania) |
| STAS 791(88) 34MoCr11 (Romania) |
| STAS 791(88) 34MoCr11S (Romania) |
| STAS 791(88) 34MoCr11X (Romania) |
| STAS 791(88) 34MoCr11XS (Romania) |
| GOST 4543 35ChM (Russian Federation) |
| UNE F.125 (Spain) |
| UNE F.125A (Spain) |
| UNE 36012(75) 35CrMo4 (Spain) |
| UNE 36012(75) 35CrMo4-1 (Spain) |
| UNE 36012(75) 38CrMo4 (Spain) |
| UNE 36012(75) F.1250 (Spain) |
| UNE 36012(75) F.1255 (Spain) |
| UNE 36034(85) 35CrMo4DF (Spain) |
| UNE 36034(85) F.1254 (Spain) |
| UNE 36254(79) F.8231 (Spain) |
| SIS 142234 2234-03 (Sweden) |
| SIS 142234 2234-04 (Sweden) |
| SIS 142234 2234-05 (Sweden) |
| SS 142234 2234 (Sweden) |
| ISO R683-4 26 (International) |
| BS 970/1(83) 708A37 (United Kingdom) |
| BS 970/1(83) 708H37 (United Kingdom) |
| AMS 6352 4135 (USA) |
| AMS 6365 4135 (USA) |
| AMS 6365C 4135 (USA) |
| AMS 6372 4135 (USA) |
| AMS 6372C 4135 (USA) |
| ASTM A29/A29M(93) 4135 (USA) |
| ASTM A372/372M(95) Grade F (USA) |
| ASTM A372/372M(95) Type V Grade 2 (USA) |
| ASTM A519(96) 4135 (USA) |
| ASTM A829/A829M(95) 4135 (USA) |
| DoD-F-24669/1(86) 4135 (USA) |
| MIL-S-16974E(86) 4135 (USA) |
| MIL-S-18733A(56) 4135 (USA) |
| MIL-T-6735A – – – (USA) |
| SAE 770(84) 4135 (USA) |
| SAE J404(94) 4135 (USA) |
| AISI 4135 (USA) |
| COPANT 334 4135 (Venezuela) |
| COPANT 514 4135 (Venezuela) |
| C.4731 (Yugoslavia) |
| C.4783 (Yugoslavia) |
• Argentina:
IRAM 4133 to IAS, IRAM 4137 to IAS
• Belgium:
34CrMo4 to NBN 253-02, 41CrMo4 to NBN 253-02
• Bulgaria:
35ChM to BDS 6354
• Finland:
Co.35Cr1.1Mo0.20 to SFS 459
• France:
34CD4 to AFNOR NF A35-552, 34CD4 to AFNOR NF A35-556, 34CrMo4RR to AFNOR NF A36-102, 35CD4 to AFNOR NF A35-552, 35CD4 to AFNOR NF A35-553, 35CD4 to AFNOR NF A35-556, 38CD4 to AFNOR NF A35-552, 38CD4 to AFNOR NF A35-557
• Germany:
1.7220 to DIN 1652, 1.7220 to DIN EN 10083, 1.7226 to DIN 1652, 34CrMo4 to DIN EN 10083, 34CrMoS4 to DIN 1652, 35CrMo4 to DIN
• Hungary:
CMo3 to MSZ 61, CMo3E to MSZ 61, CMo3Z to MSZ 6251
• International:
34CrMo4 to ISO 683-1, 34CrMo4 to ISO 683-18, 34CrMo4E to ISO 4954, 34CrMoS4 to ISO 683-1, 34CrMoS4 to ISO 683-18, Type 2a to ISO 683-4, Type 2b to ISO 683-4
• Italy:
34CrMo4KB to UNI 7356, 35CrMo4 to UNI 6403, 35CrMo4 to UNI 7845, 35CrMo4KB to UNI 7356, 38CrMo4 to UNI 5333, 38CrMo4KB to UNI 7356
• Japan:
SCM 3 to JIS G4105
• Mexico:
4135 to NMX-B-203-SCFI, 4135 to NMX-B-300, 4135H to NMX-B-268, 4135H to NMX-B-300, 4137 to NMX-B-203-SCFI, 4137 to NMX-B-300, 4137H to NMX-B-268, 4137H to NMX-B-300
• Norway:
CrMoII to NS
• Pan America:
4135 to COPANT 334, 4135 to COPANT 514, 4137 to COPANT 514
• Romania:
34MoCr11 to STAS 791, 34MoCr11S to STAS 791, 34MoCr11X to STAS 791, 34MoCr11XS to STAS 791, T34MoCr09 to STAS 1773
• Serbia and Montenegro:
C.4731, C.4781, C.4783
• South Korea:
SCM 435 H to KS D 3754
• Spain:
35CrMo4 to UNE 36012, 35CrMo4-1 to UNE 36012, 35CrMo4DF to UNE 36034, 38CrMo4 to UNE 36012, F.1250 to UNE 36012, F.1253 to UNE 36012, F.1254 to UNE 36034, F.1255 to UNE 36012
• Sweden:
2234 to SS 142234
• UK:
34CrMo4 to BS EN 10083-1, 34CrMo4 to BS EN 10132-3, 34CrMo4 to BS EN 10250-3, 34CrMo4 to BS EN 10297-1, 34CrMoS4 to BS EN 10083-1, 5/1 to BS 3111/1
• USA:
4135, 4135 to ASTM A29/A29M, 4135 to ASTM A519, 4135 to ASTM A829/A829M, 4135 to DoD-F-24669/1, 4135 to MIL-S-16974E, 4135 to MIL-S-18733A, 4135 to SAE J404, 4135 to SAE J770, 4137, 4137 to ASTM A29/A29M, 4137 to ASTM A331-95, 4137 to ASTM A519, 4137 to ASTM A829/A829M, 4137 to SAE J404, 4137 to SAE J770, G41350 to ASTM A1031, G41370 to ASTM A1031, Grade F Class 55 to ASTM A372/A372M, Grade F Class 65 to ASTM A372/A372M, Grade F Class 70 to ASTM A372/A372M, L72 to ASTM A320/A320M, L7B to ASTM A320/A320M, MIL-T-6735 to MIL-T-6735A, UNS G41350, UNS G41370, UNS H41350, UNS H41370, UNS K13548