AISI 1010 Carbon Steel, Similar compositions

AISI 1010 Standards with similar compositions

Argentina: IRAM 1010 to IAS, IRAM 1011 to IAS
Australia: C1008 to AS 1446, HRC to AS 1594, ICRC to AS 1595, R1008 to AS 1442, R1008 to AS 1443, R1008 to AS 1446, Temper 4 to AS 1585 Part 2, Temper 5 to AS 1585 Part 2, Temper 6 to AS 1585 Part 2
India: 15C4 to IS 11169/1, 15C4 to IS 1570/2/1, 17C 5 to IS 1812, C15 to IS 1570/2/1, CDS-1 to IS 3074, CEW C2 to IS 2039, CEW-1 to IS 3074, Deep Drawing (DD) to IS 12367, Drawing (D) to IS 12367, ERW C2 to IS 2039, ERW-1 to IS 3074, Grade 1 to IS 1673, Grade 2 to IS 1673, Grade 2 to IS 5872, Grade 3 to IS 5872, Grade 4 to IS 7887, Grade 4 to IS 8952, Grade 5 to IS 7887, Grade 5 to IS 8952, IS 11714/2 to IS 11714/2, IS 11714/3 to IS 11714/3, IS 2255 to IS 2255, IS 8057 to IS 8057, YSt 170 Class 1 to IS 1978, YSt 210 to IS 1978
International: CC11X to ISO 4954
Italy: CB10FF to UNI 7356
Japan: SGD 2 to JIS G3108, SWRCH10R to JIS G3507, SWRCH12R to JIS G3507, SWRM 10 to JIS G3505, SWRM 12 to JIS G3505
Mexico: 1010 to NMX-B-301, 1012 to NMX-B-301, B212 to NMX-B-212, Grade A Type S to NMX-B-205, MT1010 to NMX-B-201
Pan America: 1008 to COPANT 330, 1008 to COPANT 331, 1008 to COPANT 333, 1012 to COPANT 333, EP to COPANT 38
Poland: St2N to PN-H-84022, St2N to PN-H-84023/01
Serbia and Montenegro: Z10N
South Korea: SGD 2 to KS D 3526, SWRCH10A to KS D 3592, SWRCH10R to KS D 3592, SWRCH12R to KS D 3592, SWRM 10 to KS D 3554, SWRM 12 to KS D 3554
Sweden: 1142-42 to SIS 141142, 1146-32 to SIS 141146, 1146-42 to SIS 141146
Turkey: C12-1/1.0012 to TS 2348, C9-1/1.0010 to TS 2348
UK: 045M10 to BS 970/1, HS12 to BS 1449 Section 1.14, HS15 to BS 1449 Section 1.8
USA: 040 X,Y,Z to SAE J1392, 1010, 1010 to ASTM A29/A29M, 1010 to ASTM A512-96, 1010 to ASTM A513, 1010 to ASTM A519, 1010 to ASTM A568/A568M, 1010 to ASTM A787, 1010 to SAE J403, 1012, 1012 to ASTM A29/A29M, 1012 to ASTM A512-96, 1012 to ASTM A513, 1012 to ASTM A519, 1012 to ASTM A568/A568M, 1012 to MIL-R-8814, 1012 to SAE J403, A179 to ASTM A179/A179M, A2 to ASTM A556/A556M-96, A214 to ASTM A214/A214M, A254 to ASTM A254, A822 to ASTM A822/A822M, C1 to MIL-S-16788A, G10100 to ASTM A510/A510M, G10100 to ASTM A576-90b, G10100 to ASTM A830/A830M, G10120 to ASTM A510/A510M, G10120 to ASTM A576-90b, G10120 to ASTM A830/A830M, Grade A ERW to ASTM A523-96, Grade A Seamless to ASTM A523-96, Grade A to ASTM A1020/A1020M, Grade A to ASTM A178/A178M, Grade B to ASTM A285/A285M, M1010, M1010 to ASTM A29/A29M, M1010 to ASTM A575-96, M1010 to SAE J403, M1012, M1012 to ASTM A29/A29M, M1012 to ASTM A575-96, M1012 to SAE J403, MT1010 to ASTM A512-96, MT1010 to ASTM A513, MT1010 to ASTM A519, MT1010 to ASTM A787, SAE J356 to SAE J356, SAE J524 to SAE J524, SAE J525 to SAE J525, UNS G10100, UNS G10120, UNS K01001, UNS K01200, UNS K01807, UNS K02200, UNS K02201
Tradenames: AIRCO S-10, ASCOMETAL XC10, B&W CARBON STEEL, FORTUNA WO 3, GRANIT 1, KRUPP STE 280 Z, KRUPP STE 280-2 Z, KRUPP STE 280-3 Z, KRUPP UQST 38, KRUPP UST 38, MCKAY 19, NAPAC-35, NAPAC-40, NAPAC-45, NAPAC-50, POMPEY FFC 1, RACO 5, RACO RED LABEL, S-1010, SHARALLOY, SHARALLOY 45, UNA NO. 200, UNA NO. 3200, USS 1110, VERTOMAR 10, VV, WITTEN W 01 E

Designation

Carbon steel: AISI 1010 (annealed)
ConditionAnnealed
UNS numberG10100
US nameSAE J527, ASTM MT 1010, ASTM M1012, ASTM M1010, ASTM 130, ASTM 1012, ASTM 1010, ASME G10120, ASME G10100, ~SAE SAE J526, ~ASTM M1008, ~ASTM G10130, ~AMS 5053
EN nameHS12, ~HS4, ~ERW101, ~DC03, ~DC01
EN number~1.1207, ~1.1121, ~1.0357, ~1.0347, ~1.0330
ISO nameCC8X, CC8A, CC11X, CC11A, ~HR1, ~CR2, ~CE10
GB (Chinese) nameML10Al, ML08Al, ~Q215, ~CRB550
JIS (Japanese) nameSGD 2, ~SPCC, ~SGD 1, ~SBC 300

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey