AISI 1010 Carbon Steel Annealed Mechanical Properties

Young’s modulus205–215GPa
Specific stiffness26.1–27.4MN.m/kg
Yield strength (elastic limit)172–315MPa
Tensile strength310–430MPa
Specific strength21.9–40.1kN.m/kg
Elongation29–45% strain
Compressive strength255–315MPa
Flexural modulus205–215GPa
Flexural strength (modulus of rupture)255–315MPa
Shear modulus79–84GPa
Bulk modulus158–175GPa
Poisson’s ratio0.285–0.295 
Shape factor64   
Hardness – Vickers88–128HV
Hardness – Rockwell B42  HRB
Elastic stored energy (springs)75.6–220kJ/m^3
Fatigue strength at 10^7 cycles203–238MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles160–302MPa

Impact & fracture properties: AISI 1010 Carbon Steel Annealed

Fracture toughness43–69           MPa.m^0.5
Toughness (G)9.21–21.7kJ/m^2

Carbon steel, AISI 1010, annealed

Designation

Carbon steel: AISI 1010 (annealed)
ConditionAnnealed
UNS numberG10100
US nameSAE J527, ASTM MT 1010, ASTM M1012, ASTM M1010, ASTM 130, ASTM 1012, ASTM 1010, ASME G10120, ASME G10100, ~SAE SAE J526, ~ASTM M1008, ~ASTM G10130, ~AMS 5053
EN nameHS12, ~HS4, ~ERW101, ~DC03, ~DC01
EN number~1.1207, ~1.1121, ~1.0357, ~1.0347, ~1.0330
ISO nameCC8X, CC8A, CC11X, CC11A, ~HR1, ~CR2, ~CE10
GB (Chinese) nameML10Al, ML08Al, ~Q215, ~CRB550
JIS (Japanese) nameSGD 2, ~SPCC, ~SGD 1, ~SBC 300

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey