AISI 1010 Carbon Steel Annealed Mechanical Properties
AISI 1010 Carbon Steel Annealed Mechanical Properties Young’s modulus 205 – 215 GPa Specific stiffness 26.1 – 27.4 MN.m/kg Yield strength (elastic limit) 172 – 315 MPa Tensile strength 310 – 430 MPa Specific strength 21.9 – 40.1 kN.m/kg Elongation 29 – 45 % strain Compressive strength 255 – 315 MPa Flexural modulus 205 – … Continue reading AISI 1010 Carbon Steel Annealed Mechanical Properties