EN GJN HV600 (XCr11) Chemical Composition, former BS 3F, Cast iron, white, high-chromium alloy

Compositional summary

Fe73-87 / Cr11-14 / C1.8-3.6 / Mn0.15-1.5 (impurities: Mo<3, Cu<2, Ni<2, Si<1, P<0.1, S<0.1)

Material family: Metal (ferrous)

Base material: Fe (Iron)

ElementsMinMax%
C (carbon) 1.8–3.6%
Cr (chromium) 11–14%
Cu (copper) 0–2%
Fe (iron) 72.8–87.1%
Mn (manganese) 0.15–1.5%
Mo (molybdenum) 0–3%
Ni (nickel) 0–2%
P (phosphorus) 0–0.1%
S (sulfur) 0–0.1%
Si (silicon) 0–1%
EN GJN HV600 (XCr11) Chemical Composition, former BS 3F, Cast iron, white, high-chromium alloy