AISI 12L14 Leaded Resulfurized Low Carbon Steel

AISI 12L14 Leaded Resulfurized Low Carbon Steel

AISI 12L14 Steel Overview

AISI 12L14 steel (UNS G12144, EN 11SMnPb37) is a leaded resulfurized low carbon steel. AISI 12L14 is a free-machining grade: its raised sulfur and lead content gives short chips and fast cutting speeds. This page lists the AISI 12L14 material data sheets for 1 condition: as rolled. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 12L14 Steel

Free-machining / free-cutting steel for automatic screw machine and tool products, shafts, bolts, fasteners, cams, lightly stressed fasteners, for the automotive and general engineering industries.

AISI 12L14 Steel Chemical Composition

C (carbon)0 – 0.15 %
Fe (iron)97.8 – 98.7 %
Mn (manganese)0.85 – 1.15 %
P (phosphorus)0.04 – 0.09 %
Pb (lead)0.15 – 0.35 %
S (sulfur)0.26 – 0.35 %
Si (silicon)0 – 0.1 %

AISI 12L14 Steel Material Data Sheets

AISI 12L14 As Rolled Material Data Sheet

AISI 12L14 Compared with Other Resulfurized Steels

Compare the composition, mechanical properties and machining speed of AISI 12L14 with AISI 1117, 1118, 12L14, 1137, 1141 and 1144 in our resulfurized free-machining steels comparison.

AISI 12L14 Steel Parts from Turkey

Looking for AISI 12L14 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 12L14 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low carbon steel grades.