AISI 1015 Annealed vs As Rolled vs Normalized: Yield, Tensile & Hardness Compared

How do the AISI 1015 heat treatment properties change from one condition to another? This comparison puts the yield strength, tensile strength, hardness, elongation and machining speed of AISI 1015 low carbon steel (UNS G10150) side by side for 3 conditions: annealed, as rolled, normalized. All values are taken from the individual AISI 1015 material data sheets linked below.

AISI 1015 Yield, Tensile and Hardness by Condition

ConditionYield strength (MPa)Tensile strength (MPa)Hardness (HV)Elongation (%)Machining speed (m/min)
Annealed255–315345–430108–12829–4545.7
As Rolled280–345375–465123–14331–4739.6
Normalized300–355380–470118–13829–4542.7

AISI 1015 Differences Compared with Annealed

The table below shows how much each AISI 1015 condition differs from the annealed condition, based on the mid-point of each range. Positive values mean higher strength, hardness or elongation.

ConditionYield strengthTensile strengthHardnessElongation
As Rolled+10%+8%+13%+5%
Normalized+15%+10%+8%+0%

AISI 1015 Strength and Hardness Charts

AISI 1015 Yield strength by condition (MPa)Annealed255–315As Rolled280–345Normalized300–355
AISI 1015 Tensile strength by condition (MPa)Annealed345–430As Rolled375–465Normalized380–470
AISI 1015 Hardness by condition (HV)Annealed108–128As Rolled123–143Normalized118–138

AISI 1015 Heat Treatment Key Points

The highest tensile strength of AISI 1015 in these data sheets is reached in the normalized condition (380–470 MPa). The softest condition is annealed (108–128 HV), with a machining speed of 45.7 m/min, which is usually preferred for machining and forming.

AISI 1015 Material Data Sheets

AISI 1015 Annealed | AISI 1015 As Rolled | AISI 1015 Normalized | All AISI 1015 conditions

Looking for AISI 1015 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1015 steel parts in-house, heat treated to the condition you specify, and inspects them before shipment.