How do the AISI 1015 heat treatment properties change from one condition to another? This comparison puts the yield strength, tensile strength, hardness, elongation and machining speed of AISI 1015 low carbon steel (UNS G10150) side by side for 3 conditions: annealed, as rolled, normalized. All values are taken from the individual AISI 1015 material data sheets linked below.
AISI 1015 Yield, Tensile and Hardness by Condition
| Condition | Yield strength (MPa) | Tensile strength (MPa) | Hardness (HV) | Elongation (%) | Machining speed (m/min) |
|---|---|---|---|---|---|
| Annealed | 255–315 | 345–430 | 108–128 | 29–45 | 45.7 |
| As Rolled | 280–345 | 375–465 | 123–143 | 31–47 | 39.6 |
| Normalized | 300–355 | 380–470 | 118–138 | 29–45 | 42.7 |
AISI 1015 Differences Compared with Annealed
The table below shows how much each AISI 1015 condition differs from the annealed condition, based on the mid-point of each range. Positive values mean higher strength, hardness or elongation.
| Condition | Yield strength | Tensile strength | Hardness | Elongation |
|---|---|---|---|---|
| As Rolled | +10% | +8% | +13% | +5% |
| Normalized | +15% | +10% | +8% | +0% |
AISI 1015 Strength and Hardness Charts
AISI 1015 Heat Treatment Key Points
The highest tensile strength of AISI 1015 in these data sheets is reached in the normalized condition (380–470 MPa). The softest condition is annealed (108–128 HV), with a machining speed of 45.7 m/min, which is usually preferred for machining and forming.
AISI 1015 Material Data Sheets
AISI 1015 Annealed | AISI 1015 As Rolled | AISI 1015 Normalized | All AISI 1015 conditions