Home » PA (Polyamide / Nylon) » PA12 (Polyamide 12 / Nylon 12) » PA12 Unfilled Grades » PA12 Rigid Grade Material Data Sheet
PA12 Rigid Grade (Polyamide 12) Material Data Sheet
PA12 Rigid Grade Overview
PA12 rigid grade is a grade of polyamide 12 (PA12, nylon 12), designated Polyamide (Nylon) (Type 12, Molding and Extrusion). This PA12 rigid grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA12 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA12 parts in-house and inspects them before shipment.
PA12 Rigid Grade Designation
Polyamide (Nylon) (Type 12, Molding and Extrusion) Tradenames Ashlene, Badamid, Dynastat, Fostalon, Fostamid, Gravi-Tech, Grilamid, Hifill, Latimass, Luvocom, Pentamid, Plustek, Rilsamid, Rilsan, Schulamid, Therma-Tech, Ubesta, Vestamid, Vestosint
PA12 Rigid Grade Typical uses
Precision engineering components, components requiring low temperature toughness, sports shoe soles.
PA12 Rigid Grade Composition detail
PA12 Rigid Grade Physical properties
PA12 Rigid Grade Mechanical properties
Young’s modulus 1.08 – 1.35 GPa Specific stiffness 1.07 – 1.34 MN.m/kg Yield strength (elastic limit) 34.8 – 43.4 MPa Tensile strength 45 – 55 MPa Specific strength 34.4 – 43 kN.m/kg Elongation 41 – 59 % strain Elongation at yield 7.03 – 13.3 % strain Compressive modulus 1.08 – 1.35 GPa Compressive strength 57 – 63 MPa Flexural modulus 1.17 – 1.2 GPa Flexural strength (modulus of rupture) 57.4 – 70.1 MPa Shear modulus 0.418 – 0.439 GPa Shear strength 27 – 33 MPa Bulk modulus 2.47 – 2.74 GPa Poisson’s ratio 0.406 – 0.422 Shape factor 4.19 Hardness – Vickers 11 – 12 HV Hardness – Rockwell M 70 – 80 Hardness – Rockwell R 100 – 110 Hardness – Brinell 62 – 78 HB Hardness – Shore D 69 – 71 Elastic stored energy (springs) 496 – 789 kJ/m3 Fatigue strength at 10^7 cycles 19 – 21 MPa
PA12 Rigid Grade Impact & fracture properties
Fracture toughness 3.18 – 3.52 MPa.m0.5 Toughness (G) 8.01 – 10.7 kJ/m2 Impact strength, notched 23 °C 15.1 – 29.3 kJ/m2 Impact strength, notched -30 °C 5.04 – 11 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
PA12 Rigid Grade Thermal properties
Melting point 170 – 178 °C Glass temperature 40 – 43 °C Heat deflection temperature 0.45MPa 70 – 94 °C Heat deflection temperature 1.8MPa 35 – 57 °C Maximum service temperature 80 – 110 °C Minimum service temperature -67 – -47 °C Thermal conductivity 0.218 – 0.306 W/m.°C Specific heat capacity 1680 – 1720 J/kg.°C Thermal expansion coefficient 110 – 180 µstrain/°C Thermal shock resistance 173 – 304 °C Thermal distortion resistance 0.00138 – 0.00245 MW/m
PA12 Rigid Grade Electrical properties
Electrical resistivity 2.81e19 – 7.03e20 µohm.cm Electrical conductivity 2.45e-19 – 6.14e-18 %IACS Dielectric constant (relative permittivity) 4.2 – 5.92 Dissipation factor (dielectric loss tangent) 0.0473 – 0.125 Dielectric strength (dielectric breakdown) 23.4 – 39.8 MV/m Comparative tracking index 600 V
PA12 Rigid Grade Magnetic properties
Magnetic type Non-magnetic
PA12 Rigid Grade Optical, aesthetic and acoustic properties
Refractive index 1.52 – 1.54 Transparency Translucent Acoustic velocity 1030 – 1160 m/s Mechanical loss coefficient (tan delta) 0.02 – 0.07
PA12 Rigid Grade Absorption & permeability
Water absorption @ 24 hrs 0.53 – 0.87 % Water absorption @ sat 1.4 – 1.8 % Humidity absorption @ sat 0.62 – 0.84 % Water vapor transmission 0.35 g.mm/m².day Permeability (O2) 35 cm³.mm/m².day.atm
PA12 Rigid Grade Processing properties
Polymer injection molding Excellent Polymer extrusion Acceptable Polymer thermoforming Limited use Linear mold shrinkage 0.8 – 1.5 % Melt temperature 177 – 274 °C Mold temperature 40 – 60 °C Molding pressure range 16 – 75 MPa
PA12 Rigid Grade Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Limited use Organic solvents Acceptable Oils and fuels Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Highly flammable
PA12 Grades
PA12 Unfilled Material Data Sheets
Other PA12 grades:
All PA12 Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey