Home » PA (Polyamide / Nylon) » PA612 (Polyamide 612 / Nylon 612) » PA612 Glass Filled Grades » PA612 30% Glass Fiber Flame Retarded Material Data Sheet
PA612 30% Glass Fiber Flame Retarded (Polyamide 612) Material Data Sheet
PA612 30% Glass Fiber Flame Retarded Overview
PA612 30% glass fiber flame retarded is a grade of polyamide 612 (PA612, nylon 612), designated Polyamide (Nylon) (Type 612, 30% Glass Fiber, Flame Retarded). This PA612 30% glass fiber flame retarded material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.
PA612 30% Glass Fiber Flame Retarded Designation
Polyamide (Nylon) (Type 612, 30% Glass Fiber, Flame Retarded) Tradenames Akromid, Edgetek, Grilamid, Technyl, Ultramid, Zytel
PA612 30% Glass Fiber Flame Retarded Typical uses
Mechanical parts, zips, filaments, coverings and coatings requiring abrasion resistance.
PA612 30% Glass Fiber Flame Retarded Composition detail
Polymer 55 – 65 % Flame retardant 5 – 15 % Glass (fiber) 30 %
PA612 30% Glass Fiber Flame Retarded Physical properties
PA612 30% Glass Fiber Flame Retarded Mechanical properties
Young’s modulus 8.96 – 11.2 GPa Specific stiffness 6.89 – 8.62 MN.m/kg Yield strength (elastic limit) 125 – 155 MPa Tensile strength 126 – 154 MPa Specific strength 96.1 – 119 kN.m/kg Elongation 2.31 – 3.32 % strain Elongation at yield 1.94 – 3.69 % strain Compressive modulus 9.57 – 10.6 GPa Compressive strength 160 – 176 MPa Flexural modulus 7.88 – 9.44 GPa Flexural strength (modulus of rupture) 188 – 229 MPa Shear modulus 3.59 – 3.77 GPa Shear strength 75.6 – 92.4 MPa Bulk modulus 12.1 – 13.3 GPa Poisson’s ratio 0.354 – 0.368 Shape factor 6.59 Hardness – Vickers 40 – 44 HV Hardness – Rockwell M 170 – 188 Hardness – Rockwell R 170 – 188 Hardness – Shore D 95 – 99 Elastic stored energy (springs) 770 – 1210 kJ/m3 Fatigue strength at 10^7 cycles 53.2 – 58.8 MPa
PA612 30% Glass Fiber Flame Retarded Impact & fracture properties
Fracture toughness 4.88 – 5.39 MPa.m0.5 Toughness (G) 2.27 – 3.04 kJ/m2 Impact strength, notched 23 °C 10.2 – 19.8 kJ/m2 Impact strength, notched -30 °C 6.3 – 13.7 kJ/m2 Impact strength, unnotched 23 °C 64.8 – 95.2 kJ/m2 Impact strength, unnotched -30 °C 42 – 63 kJ/m2
PA612 30% Glass Fiber Flame Retarded Thermal properties
Melting point 195 – 217 °C Glass temperature 40 – 52 °C Heat deflection temperature 0.45MPa 182 – 228 °C Heat deflection temperature 1.8MPa 174 – 220 °C Maximum service temperature 90 – 120 °C Minimum service temperature -127 – -107 °C Thermal conductivity 0.436 – 0.453 W/m.°C Specific heat capacity 1340 – 1400 J/kg.°C Thermal expansion coefficient 48.9 – 49.9 µstrain/°C Thermal shock resistance 242 – 327 °C Thermal distortion resistance 0.00879 – 0.00919 MW/m
PA612 30% Glass Fiber Flame Retarded Electrical properties
Electrical resistivity 2.73e21 – 6.83e22 µohm.cm Electrical conductivity 2.52e-21 – 6.32e-20 %IACS Dielectric constant (relative permittivity) 4.57 – 6.44 Dissipation factor (dielectric loss tangent) 0.0223 – 0.0587 Dielectric strength (dielectric breakdown) 20.4 – 34.7 MV/m Comparative tracking index 600 V
PA612 30% Glass Fiber Flame Retarded Magnetic properties
Magnetic type Non-magnetic
PA612 30% Glass Fiber Flame Retarded Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2620 – 2940 m/s Mechanical loss coefficient (tan delta) 0.00854 – 0.00944
PA612 30% Glass Fiber Flame Retarded Absorption & permeability
Water absorption @ 24 hrs 0.11 – 0.19 % Water absorption @ sat 1.7 – 2.2 % Humidity absorption @ sat 0.7 – 0.95 %
PA612 30% Glass Fiber Flame Retarded Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.2 – 0.5 % Melt temperature 213 – 288 °C Mold temperature 30 – 60 °C Molding pressure range 27.5 – 138 MPa
PA612 30% Glass Fiber Flame Retarded Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Self-extinguishing