Home » PA (Polyamide / Nylon) » PA612 (Polyamide 612 / Nylon 612) » PA612 Unfilled Grades » PA612 Toughened Grade Material Data Sheet
PA612 Toughened Grade (Polyamide 612) Material Data Sheet
PA612 Toughened Grade Overview
PA612 toughened grade is a grade of polyamide 612 (PA612, nylon 612), designated Polyamide (Nylon) (Type 612, Unreinforced, Toughened). This PA612 toughened grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.
PA612 Toughened Grade Designation
Polyamide (Nylon) (Type 612, Unreinforced, Toughened) Tradenames Schulamid, Vestamid
PA612 Toughened Grade Typical uses
Mechanical parts, zips, filaments, coverings and coatings requiring abrasion resistance.
PA612 Toughened Grade Composition detail
Polymer 85 – 97 % Impact modifier 3 – 15 %
PA612 Toughened Grade Physical properties
PA612 Toughened Grade Mechanical properties
Young’s modulus 0.49 – 0.611 GPa Specific stiffness 0.485 – 0.605 MN.m/kg Yield strength (elastic limit) 19.6 – 24.4 MPa Tensile strength 24.8 – 30.3 MPa Specific strength 19.4 – 24.2 kN.m/kg Elongation 55.4 – 79.7 % strain Elongation at yield 24.2 – 45.9 % strain Compressive modulus 0.523 – 0.578 GPa Compressive strength 31.4 – 34.7 MPa Flexural modulus 0.735 – 0.88 GPa Flexural strength (modulus of rupture) 24.8 – 30.3 MPa Shear modulus 0.189 – 0.198 GPa Shear strength 14.9 – 18.2 MPa Bulk modulus 1.12 – 1.23 GPa Poisson’s ratio 0.405 – 0.422 Shape factor 3.8 Hardness – Vickers 6 – 7 HV Hardness – Rockwell M 69 – 76 Hardness – Rockwell R 69 – 76 Hardness – Shore D 66 – 69 Elastic stored energy (springs) 347 – 550 kJ/m3 Fatigue strength at 10^7 cycles 10.5 – 11.6 MPa
PA612 Toughened Grade Impact & fracture properties
Fracture toughness 2.71 – 3 MPa.m0.5 Toughness (G) 12.8 – 17.2 kJ/m2 Impact strength, notched 23 °C 54.4 – 106 kJ/m2 Impact strength, notched -30 °C 8.19 – 17.8 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
PA612 Toughened Grade Thermal properties
Melting point 195 – 217 °C Glass temperature 40 – 52 °C Heat deflection temperature 0.45MPa 66 – 100 °C Heat deflection temperature 1.8MPa 41 – 74 °C Maximum service temperature 42 – 57 °C Minimum service temperature -127 – -107 °C Thermal conductivity 0.213 – 0.222 W/m.°C Specific heat capacity 1710 – 1780 J/kg.°C Thermal expansion coefficient 167 – 170 µstrain/°C Thermal shock resistance 204 – 277 °C Thermal distortion resistance 0.00127 – 0.00132 MW/m
PA612 Toughened Grade Electrical properties
Electrical resistivity 2.46e21 – 6.15e22 µohm.cm Electrical conductivity 2.8e-21 – 7.01e-20 %IACS Dielectric constant (relative permittivity) 4.26 – 6.01 Dissipation factor (dielectric loss tangent) 0.0431 – 0.114 Dielectric strength (dielectric breakdown) 23.5 – 40.1 MV/m Comparative tracking index 600 V
PA612 Toughened Grade Magnetic properties
Magnetic type Non-magnetic
PA612 Toughened Grade Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 695 – 779 m/s Mechanical loss coefficient (tan delta) 0.028 – 0.0309
PA612 Toughened Grade Absorption & permeability
Water absorption @ 24 hrs 0.54 – 0.88 % Water absorption @ sat 2.4 – 3.1 % Humidity absorption @ sat 1 – 1.4 % Permeability (O2) 36.5 – 86 cm³.mm/m².day.atm
PA612 Toughened Grade Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 1 – 1.21 % Melt temperature 213 – 288 °C Mold temperature 30 – 60 °C Molding pressure range 6.88 – 103 MPa
PA612 Toughened Grade Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning