PA612 10% PTFE Lubricated (Polyamide 612) Material Data Sheet
PA612 10% PTFE Lubricated Overview
PA612 10% PTFE lubricated is a grade of polyamide 612 (PA612, nylon 612), designated Polyamide (Nylon) (Type 612, 10% PTFE, Lubricated). This PA612 10% PTFE lubricated material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.
PA612 10% PTFE Lubricated Designation
Polyamide (Nylon) (Type 612, 10% PTFE, Lubricated) Tradenames LNP Lubricomp, Lubrione, Nycal, Plaslube, Radici, Zytel
PA612 10% PTFE Lubricated Typical uses
Mechanical parts, zips, filaments, coverings and coatings requiring abrasion resistance.
PA612 10% PTFE Lubricated Composition detail
Polymer 90 % PTFE (lubricant) 10 %
PA612 10% PTFE Lubricated Physical properties
PA612 10% PTFE Lubricated Mechanical properties
Young’s modulus 1.49 – 1.86 GPa Specific stiffness 1.34 – 1.67 MN.m/kg Yield strength (elastic limit) 43.6 – 54.4 MPa Tensile strength 52.9 – 64.7 MPa Specific strength 39.1 – 48.8 kN.m/kg Elongation 55.4 – 79.7 % strain Elongation at yield 24.2 – 45.9 % strain Compressive modulus 1.59 – 1.76 GPa Compressive strength 67 – 74.1 MPa Flexural modulus 1.58 – 1.89 GPa Flexural strength (modulus of rupture) 70.1 – 85.6 MPa Shear modulus 0.569 – 0.598 GPa Shear strength 31.7 – 38.8 MPa Bulk modulus 4.14 – 4.58 GPa Poisson’s ratio 0.42 – 0.436 Shape factor 4.4 Hardness – Vickers 14 – 15 HV Hardness – Rockwell M 110 – 121 Hardness – Rockwell R 110 – 121 Hardness – Shore D 80 – 83 Elastic stored energy (springs) 565 – 899 kJ/m3 Fatigue strength at 10^7 cycles 22.3 – 24.7 MPa
PA612 10% PTFE Lubricated Impact & fracture properties
Fracture toughness 3.4 – 3.75 MPa.m0.5 Toughness (G) 6.63 – 8.84 kJ/m2 Impact strength, notched 23 °C 5.01 – 9.72 kJ/m2 Impact strength, notched -30 °C 3.33 – 7.24 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
PA612 10% PTFE Lubricated Thermal properties
Melting point 195 – 217 °C Glass temperature 40 – 52 °C Heat deflection temperature 0.45MPa 102 – 140 °C Heat deflection temperature 1.8MPa 77 – 113 °C Maximum service temperature 90 – 120 °C Minimum service temperature -127 – -107 °C Thermal conductivity 0.185 – 0.192 W/m.°C Specific heat capacity 1600 – 1660 J/kg.°C Thermal expansion coefficient 99 – 101 µstrain/°C Thermal shock resistance 251 – 341 °C Thermal distortion resistance 0.00184 – 0.00192 MW/m
PA612 10% PTFE Lubricated Electrical properties
Electrical resistivity 2.46e21 – 6.15e22 µohm.cm Electrical conductivity 2.8e-21 – 7.01e-20 %IACS Dielectric constant (relative permittivity) 4.26 – 6.01 Dissipation factor (dielectric loss tangent) 0.0428 – 0.113 Dielectric strength (dielectric breakdown) 23.5 – 40.1 MV/m Comparative tracking index 600 V
PA612 10% PTFE Lubricated Magnetic properties
Magnetic type Non-magnetic
PA612 10% PTFE Lubricated Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 1150 – 1290 m/s Mechanical loss coefficient (tan delta) 0.0191 – 0.0211
PA612 10% PTFE Lubricated Absorption & permeability
Water absorption @ 24 hrs 0.48 – 0.79 % Water absorption @ sat 2.1 – 2.8 % Humidity absorption @ sat 0.9 – 1.2 %
PA612 10% PTFE Lubricated Processing properties
Polymer injection molding Excellent Polymer extrusion Unsuitable Polymer thermoforming Limited use Linear mold shrinkage 1.09 – 1.32 % Melt temperature 213 – 288 °C Mold temperature 30 – 60 °C Molding pressure range 27.5 – 138 MPa
PA612 10% PTFE Lubricated Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning