PA610 Glass Filled Grades

PA610 Glass Filled Grades

PA610 Glass Filled Grades Overview

PA610 glass filled grades are polyamide 610 (nylon 610) compounds grouped by their reinforcement and additives. Glass fiber reinforcement raises tensile strength, stiffness, creep resistance and heat deflection temperature and reduces thermal expansion. Long-fiber grades add further impact strength, while flame-retarded, toughened and lubricated versions target specific applications. The PA610 glass filled material data sheets below list designation, composition, physical, mechanical, thermal and electrical properties for each grade. Looking for PA610 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA610 parts in-house and inspects them before shipment.

PA610 Glass Filled Material Data Sheets

PA610 30-40% Glass Fiber Material Data Sheet

More PA610 Grades

All PA610 grades | PA610 Unfilled Grades