PA610 (nylon 610) absorbs roughly half as much water as PA6 and PA66, which gives better dimensional stability and steadier electrical properties. It stays tough to very low temperatures and is stronger than PA6/12, PA12 and PA11.
PA610 Limitations
Strength is lower than PA6 or PA66, cost is higher, and mold shrinkage is high.
PA610 Designation
PA610, also written 6.10 or 6/10.
Typical Uses of PA610
Electrical insulation and components similar to those made from PA6 and PA66 where lower moisture uptake justifies the higher price, such as zip fasteners, insulators, precision parts and brush filaments.
PA610 Compositional Summary
(NH(CH2)6NHCO(CH2)8CO)n. The renewable part comes from sebacic acid, obtained from castor oil.
Material family
Plastic (thermoplastic, semi-crystalline)
Base material
PA610 (Polyamide / nylon 610)
CAS number
9011-52-3