Home » PA (Polyamide / Nylon) » PA66 (Polyamide 66 / Nylon 66) » PA66 Stainless Steel Filled Grades » PA66 10% Stainless Steel Long Fiber Material Data Sheet
PA66 10% Stainless Steel Long Fiber (Polyamide 66) Material Data Sheet
PA66 10% Stainless Steel Long Fiber Overview
PA66 10% stainless steel long fiber is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 10% Stainless Steel Long Fiber, Conductive – EMI Shielding). This PA66 10% stainless steel long fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.
PA66 10% Stainless Steel Long Fiber Designation
Polyamide (Nylon) (Type 66, 10% Stainless Steel Long Fiber, Conductive – EMI Shielding) Tradenames Celstran
PA66 10% Stainless Steel Long Fiber Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA66 10% Stainless Steel Long Fiber Composition detail
Polymer 90 % Stainless steel (fiber) 10 %
PA66 10% Stainless Steel Long Fiber Physical properties
PA66 10% Stainless Steel Long Fiber Mechanical properties
Young’s modulus 1.74 – 2.17 GPa Specific stiffness 1.4 – 1.75 MN.m/kg Yield strength (elastic limit) 40 – 49.9 MPa Tensile strength 48.6 – 59.4 MPa Specific strength 32.3 – 40.3 kN.m/kg Elongation 3.8 – 5.47 % strain Elongation at yield 3.04 – 5.77 % strain Compressive modulus 1.86 – 2.06 GPa Compressive strength 61.5 – 68 MPa Flexural modulus 1.58 – 1.89 GPa Flexural strength (modulus of rupture) 60.8 – 74.4 MPa Shear modulus 0.684 – 0.719 GPa Shear strength 29.1 – 35.6 MPa Bulk modulus 2.98 – 3.3 GPa Poisson’s ratio 0.381 – 0.397 Shape factor 4.92 Hardness – Vickers 13 – 14 HV Hardness – Rockwell M 104 – 115 Hardness – Rockwell R 104 – 115 Hardness – Shore D 78 – 82 Elastic stored energy (springs) 407 – 648 kJ/m3 Fatigue strength at 10^7 cycles 20.5 – 22.7 MPa
PA66 10% Stainless Steel Long Fiber Impact & fracture properties
Fracture toughness 3.5 – 3.87 MPa.m0.5 Toughness (G) 6.03 – 8.06 kJ/m2 Impact strength, notched 23 °C 4.65 – 9.02 kJ/m2 Impact strength, notched -30 °C 3.3 – 7.18 kJ/m2
PA66 10% Stainless Steel Long Fiber Thermal properties
Melting point 257 – 265 °C Glass temperature 54 – 66 °C Heat deflection temperature 0.45MPa 126 – 167 °C Heat deflection temperature 1.8MPa 121 – 161 °C Maximum service temperature 90 – 130 °C Minimum service temperature -81 – -71 °C Thermal conductivity 0.301 – 0.313 W/m.°C Specific heat capacity 1500 – 1560 J/kg.°C Thermal expansion coefficient 91.8 – 93.6 µstrain/°C Thermal shock resistance 213 – 289 °C Thermal distortion resistance 0.00324 – 0.00338 MW/m
PA66 10% Stainless Steel Long Fiber Electrical properties
Electrical resistivity 10000 – 1e6 µohm.cm Electrical conductivity 1.72e-4 – 0.0172 %IACS Galvanic potential -0.14 – -0.06 V
PA66 10% Stainless Steel Long Fiber Magnetic properties
PA66 10% Stainless Steel Long Fiber Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 1180 – 1330 m/s Mechanical loss coefficient (tan delta) 0.0191 – 0.0211
PA66 10% Stainless Steel Long Fiber Absorption & permeability
Water absorption @ 24 hrs 0.55 – 0.9 % Water absorption @ sat 6.3 – 8.4 % Humidity absorption @ sat 1.8 – 2.5 %
PA66 10% Stainless Steel Long Fiber Processing properties
Polymer injection molding Limited use Polymer extrusion Unsuitable Polymer thermoforming Limited use Linear mold shrinkage 0.3 – 0.4 % Melt temperature 223 – 299 °C Molding pressure range 34.4 – 138 MPa
PA66 10% Stainless Steel Long Fiber Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Poor Flammability Slow-burning
PA66 Grades
PA66 Stainless Steel Filled Material Data Sheets
All PA66 Grades
Modulus Metal Services